When 2A12 aluminum plate is processed into a workpiece, sometimes the surface will adhere to some unclean solution, if the 2A12 aluminum plate solution cleaning will cause a certain impact, then 2A12 aluminum plate manufacturer will introduce to you, the impact of 2A12 aluminum plate workpiece cleaning.

2A12 aluminum workpieces are not washed thoroughly after alkali washing.The lye in the hole cannot be washed clean. After the oxidation technology, the lye will promote the eye of the cylinder to flow out, resulting in the serious erosion of the oxide film near the hole.

When the lye of 2A12 aluminum plate is replaced, too many aluminum ions will accumulate after the lye is used for a long time, and it is more difficult for the aluminum ions to eluate on the surface of the workpiece of 2A12 aluminum plate, thus affecting the contact between the surface of the workpiece of 2A12 aluminum plate and the conductive oxidation liquid, thus affecting the formation of the oxide film.

2A12 very astringent aluminum self tapping screw, the operator often activated lubrication coating, if there is no emulsifier caustic solution, it is difficult to be real-time steep divisible.The holes of 2A12 aluminum plate workpiece are near the flexible shaft.

About the impact of 2A12 aluminum workpiece washing clean here, if you need 2A12 aluminum plate can contact us.