How to prevent bending of 6082 aluminum tube

Number of views:298

During the production of 6082 aluminum tube, the defect of bending may appear. How can we prevent the bending of 6082 aluminum tube during the production of 6082 aluminum tube?I'm going to introduce it to you.

1. In the case of the outer bending crack of the 6082 aluminum tube by the circular arc, the reasons should be carefully studied and analyzed to ensure that the 6082 aluminum tube has a good state of heat treatment technology. The weld of the 6082 aluminum tube can try not to be in different directions of F1 and F2 forces all the time, that is, there is no correct clamping die and bending die.After removing the pipe coefficient, check that the clamping die pressure is too high, and adjust the pressure to make it suitable.Check that the diameter of the new mandrel used is too large. When the diameter is too large, it should be required to grind the mandrel, with the mandrel of the pipe wall, and ensure good lubrication, and reduce the friction between the pipe mandrel of the anti-bending wall, and take appropriate measures to avoid rocking bed.

2. For the wrinkling of the inner arc surface, if the cut point wrinkles, the installation of the crease block, and the position of the blank block are correctly installed, and the flexible die sleeve is well matched, and the pressure of the pressurized die (wheel) can be adjusted so that the pressure of the die (wheel) can be adjusted to the appropriate pressure.If the inside of the arc is all wrinkle-free, check the diameter of the mandrel and the pitch between each node of the mandrel, or replace the mandrel.

The above is the introduction of how to prevent bending of 6082 aluminum tube during production. If you need 6082 aluminum tube, please contact us.

6082无缝铝管.jpg