We all know that if we do not pay attention to the production of 2A12 aluminum plate, pores may occur, then what impact will the generation of pores have on the performance, 2A12 aluminum plate manufacturer and how to take what measures to avoid pores?So let's go into more detail.
There are many factors affecting the generation of stomata. The generation of stomata in 2A12 aluminum plate will lead to the decline of mechanical properties of 2A12 aluminum plate and the decrease of internal tissue density. Therefore, preventive measures must be found according to the appropriate remedy for this problem.
1, first of all, we should start from the raw material, to ensure that the raw material of 2A12 aluminum plate has no impurities, fewer impurities, the possibility of pores is reduced a lot.
2, the second is to ensure that the production of 2A12 aluminum plate smelting degassing quality is better, choose a good refining and degassing agent, timely clean up the raw materials in the oxide.
3. Again, choose a good mold to ensure that the exhaust of the mold is unobstructed and the release agent is better, otherwise it will produce gas.
4, in the production process of 2A12 aluminum plate, die casting speed and temperature should be controlled.
5, try to improve the design of the mold, always pay attention to the state of the vent.
The above is about the measures to avoid the pores of 2A12 aluminum plate. If you need to consult the price of 2A12 aluminum plate, you can contact us.