The reason of the brittle pattern 5052 aluminum plate

Number of views:280

5052 aluminum plate is our common decorative pattern aluminum plate, I do not know if you have found that 5052 decorative pattern aluminum plate will appear brittle phenomenon, the next 5052 aluminum plate manufacturer will introduce to you, 5052 decorative pattern aluminum plate brittle reason.

There are three specific reasons for the brittle pattern aluminum plate:

1. Unreasonable section design of mouth shape, improper distribution of inner reinforcement and improper Angle treatment of the interface will cause stress concentration phenomenon, resulting in brittle aluminum plate with 5052 patterns. Therefore, it is necessary to improve the design to eliminate right angles and acute angles on the boundary surface.

2. When the die head pressure is insufficient, the die pressure is directly determined by the die compression ratio.In particular, the die compression ratio determined by the length of the straight line is too small, or the straight line is too short, the product becomes compact, affecting the physical performance of 5052 pattern aluminum plate aluminum roll.

3, illiquid merger and separation of rib in this case, the length of the joints should be increased and the rib, as described in the outer surface of the rib and the rib, so as to increase the compression ratio or solve the die head pressure can be changed by changing the mould plate by adjusting the length of the flow resistance, extrusion pressure mould design phase by choosing different compression ratio changes, points out that the model of the extruder screw compression ratio compression ratio, matching by adjusting the parameters of the extrusion process with change prescription 5052 aluminum design also increase the size of the molten metal can change the pressure.

The reason why 5052 pattern aluminum plate is brittle is introduced here, if you want to know more about 5052 aluminum plate information, you can contact us.