Problems encountered in cold stamping of 5052 aluminum plate and their solutions

Number of views:301

5052 aluminum plate can be used as stamping material, that in the cold processing of 5052 aluminum plate stamping, there may be a problem, the next 5052 aluminum plate manufacturer will introduce to you, 5052 aluminum plate stamping cold processing problems encountered and solutions.

1. For trimming die, because 5052 aluminum plate is relatively light, it is difficult for waste material to slide down, so it is necessary to keep the waste material smooth.

2. 5052 aluminum plate has higher requirements on the surface smoothness, perpendicularity and surface oil content of the mold.

3. The cutting edge should be as shallow as possible, and the blade gap is larger than the steel mold.

4. The maintenance and repair cost of 5052 aluminum mold is much higher than that of steel mold.

5. For drawing die, 5052 aluminum plate process is relatively more supplementary, drawing rebar is round rebar, R Angle is large.

6, for flanging die and shaping die, use as narrow as possible pressing surface, consider using air or suction method to remove the chip.

7. Mold scraps are a serious problem in the production of 5052 aluminum plate. A 2° Angle is designed on punching and trimming punch to prevent the mold from piling up and causing the die to collapse.

5052 aluminum plate cold stamping encountered problems and solutions are introduced here, if you need 5052 aluminum plate can contact us.