6061 aluminum plate is a familiar machining material, and it is also a special aluminum plate for the mold. Then the mold may or may not encounter some problems when opening the mold. Next, the 6061 aluminum plate manufacturer will share with you the problems that may be encountered when opening the mold for the 6061 aluminum plate.
1. Tolerance problems may occur in mass production.
In mass production, the mold of 6061 aluminum plate will be slightly changed and the main parameters of the press and the fluctuation of thick plate characteristics will harm the forming, which may cause changes in the specifications and surface layer. Therefore, it is necessary to strictly check and control tolerance through reasonable control methods.
(2) The problem of waste discharge.
6061 aluminum plate density is small, light weight, sometimes waste can not be discharged from the mold, very easy to spill, so a better waste ropeway.It is suggested to use reticulated plates with low friction resistance to improve the aspect ratio of the outer wall of the waste ropeway.The holes of the 6061 aluminum mold itself must also be covered with a partition to prevent the waste from flying out.
The above is about the possible problems in the mold opening of 6061 aluminum plate. If you need to know the price of 6061 aluminum plate, please contact us.