Today 6063 aluminum bar manufacturer would like to introduce to you, 6063 aluminum bar casting reference matters, hope to be helpful to you.
The production of 6063 aluminum bar through melting casting, ingot casting, flat roll rolling, heat treatment and finishing procedures.
Several key parameters in the casting process of 6063 aluminum bar:
1. During smelting, the furnace temperature is generally set at 1050℃, so the material temperature should be monitored and the surface temperature of 6063 aluminum bar should not exceed 770℃;
2, slag removal operation, the temperature of about 735℃ conducive to slag removal;
3. In general embodiments of secondary refining, the stiffening refiner is refined and the gas refining mode is used for secondary refining;
4. After standing in the inverted furnace, the casting shall be controlled within one hour; otherwise, it shall be redesigned and refined;
5. In the casting process of 6063 aluminum bar, the grain refinement of artemisinin line should be continuously added.
The above is the introduction to the smelting and casting of 6063 aluminum bar. If you need 6063 aluminum bar, please consult us.