Causes and solutions for unqualified mechanical properties of aluminum plate

Number of views:227

2024 aluminum plate is commonly used in precision machining, and its performance is required to be high. Sometimes, when we use 2024 aluminum plate, we will find that its mechanical performance is unqualified. Then, what is the cause?Are there any good solutions?Next 2024 aluminum plate manufacturers to give you a detailed.

The possible reasons are:

1, 2024 aluminum plate production temperature is too low, the temperature does not reach the solution temperature, does not play a solid solution strengthening role;

2. There are few fans at the exit of 2024 aluminum plate, and the air volume is not enough, which leads to slow cooling speed. The 2024 aluminum plate cannot be reduced below 200℃ in the shortest time, thus reducing the solid solution phase and affecting the mechanical properties of 2024 aluminum plate after heat treatment.

3. The ingot is homogenized, so that the elements in the ingot cannot be rotated again in a short time, resulting in the solid solution affecting the product performance;

4. Improper aging process and poor hot air circulation cause insufficient or over aging aging.

Solutions:

1. Reasonably and effectively control the temperature and speed during production, and keep the outlet ambient temperature of the extruder above the minimum solution temperature;

2. Strengthen the air cooling condition, and install atomization cooling device if possible to improve the cooling effect;

3. Homogenize the ingot;

4. Determine the aging process reasonably and place 2024 aluminum plate correctly to ensure smooth hot air circulation.

2024 aluminum plate mechanical properties of unqualified reasons and solutions are introduced here, if you want to understand the price of 2024 aluminum plate can consult us.