5052 aluminum plate in use, may be post-processing, sometimes is a wire drawing process and sometimes is oxidation processing, that we may not be clear about the specific difference between the two, the next 5052 aluminum plate manufacturers to introduce to you.
The wiredrawing technology of 5052 aluminum plate is as follows: the manufacturing development process of repeatedly using sandpaper to scratch out the wire of 5052 aluminum plate. The main working process of its technological research can be divided into three parts: deester, sand mill and water washing.During the wiredrawing process of 5052 aluminum plate, special coating technology after anodic treatment can be made on the surface of 5052 aluminum plate containing this metal component, and clearly show every tiny wire trace, thus making the metal matte with a fine hair luster.
The oxidation treatment of 5052 aluminum plate is: the 5052 aluminum plate is placed in the corresponding electrolyte as the anode, under the action of specific conditions and applied current, the 5052 aluminum plate is formed by electrolysis.5052 aluminum oxide film, its thickness is 5 ~ 20 microns, hard anodized film can be up to 60 ~ 200 microns.
There are many differences in the drawing of 5052 aluminum plate, which are specifically reflected in the drawing effect, corrosion resistance and pollution resistance. Sometimes, there will be oxidation parts added in the drawing process, but this is not the same as the drawing of aluminum plate is the aluminum oxide plate.
The surface of 5052 aluminum plate oxidation is the aluminum plate with oxide film, its surface and the wire drawing texture of the aluminum plate is also different, can not be confused.
The difference between 5052 aluminum plate wire drawing treatment and oxidation treatment is introduced here. If you need to know the price of 5052 aluminum sheet, you can contact us.