When 6061 aluminum plate is in use, it needs to be anodized if the customer needs it. Anodized oxidation is manually operated, after all, there may be some mistakes that lead to uneven oxide film. 6061 aluminum plate manufacturers will talk about which operation mistakes will cause uneven oxide film of 6061 aluminum plate.
1, first of all, 6061 aluminum plate workpiece alkali corrosion treatment is not thorough, oxide film, dirt failed to clean;
2. The second possibility is that there is no immediate light treatment after alkali corrosion, and the surface of 6061 aluminum plate workpiece is still alkaline.
3. It is possible that the 6061 aluminum plate workpiece came into contact with a foreign body in the process of transmission.
The above is part of the introduction of what operation errors will cause the uneven oxidation film of 6061 aluminum plate. If you want to know the price of 6061 aluminum plate, you can contact us by phone.