During the reproduction of 5083 aluminum bar, the quality of 5083 aluminum bar may deteriorate due to some reasons. Then the manufacturer of 5083 aluminum bar will give you a brief introduction about the reasons for the poor quality of 5083 aluminum bar.
The performance of 5083 aluminum bar is reduced due to the junction difference of the split rod. The length of the rod and the outer surface, the rod and the rod, or the compression ratio should be increased to solve the problem. The change of the head pressure can be adjusted by changing the length of the straight section of the head.In the mold design stage, 5083 aluminum bar can choose different compression ratio to change the extrusion pressure, but it must pay attention to the compression ratio of the head compression ratio of the extruder screw, but also can change the formula, adjust the extrusion process parameters, increase the melt pressure of the porous plate.
The mold design of 5083 aluminum bar is not reasonable, especially the distribution of inner rib and the Angle of interface.This can lead to stress concentration that needs to be improved to design and eliminate right angles and sharp angles at the interface.
The reason for the poor quality of 5083 aluminum bar is introduced here. If you want to know the price of 5083 aluminum bar, please consult us.